MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-1133 DW Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black: A-1133 BK 937 DW

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183/A
Filler Content 33 %Glass Fiber Reinforcement
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 188 MPaISO 527-2
Elongation at Break 1.7 %ISO 527-2
Tensile Modulus 11200 MPaISO 527-2
Flexural Strength 268 MPaISO 178
Flexural Modulus 10400 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180
Charpy Impact, Notched 8.20 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 296 °CUnannealed; ISO 75-2/Af
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 316 - 329 °C
Middle Barrel Temperature 316 - 329 °C
Front Barrel Temperature 324 - 335 °C
Melt Temperature 321 - 343 °C
Mold Temperature 150 °C
Drying Temperature 120 °C
Dry Time 4.00 hour
Moisture Content 0.030 - 0.060 %
 
Descriptive Properties
Agency RatingsNSF 61Tested at 82 °C (180 °F) (Commercial Hot)
AppearanceBlack
 Natural Color
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesChlorine Resistant
 Good Chemical Resistance
 Good Creep Resistance
 Good Dimensional Stability
 Good Stiffness
 High Strength
FormsPellets
GenericPPA
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant
UsesAppliances
 Consumer Applications
 Housings
 Industrial Applications
 Plumbing Parts
 Pump Parts
 Valves/Valve Parts

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® HT CESV BLACK P123 TL PA
Arkema Rilsan® HT CESV BLACK P010-HP TL PA
Arkema Rilsan® HT CESV BLACK P010 TL PA-I
Arkema Rilsan® HT CSR13 PA-CF15
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled

PSOL8Y7507 / 135588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.