MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cadi 35WS Tungsten Silver
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy; Refractory Metal; Tungsten Alloy

Material Notes: Available in a variety of rounds, rectangles, and shapes.

Information provided by Cadi Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.77 g/cc0.5336 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 80 - 8780 - 87
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000307 - 0.00000344 ohm-cm0.00000307 - 0.00000344 ohm-cm50-56 %IACS
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 35 %35 %
Tungsten, W 65 %65 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cadi 50WS Tungsten Silver
Cadi 20WS Tungsten Silver
Hogen H50S, 50 Silver/50 Tungsten PM Metal Composite
Mi-Tech Metals SW50 50 Silver/50 Tungsten PM Metal Composite
NAECO® ELKON® 1060 Silver Tungsten Carbide Contact Material

NCADI30 / 15538

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.