MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot MONARCH® 280 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: MONARCH 280 specialty carbon black is a general-purpose carbon black suitable for a variety of tinting, coloring and UV applications.

Key applications: MONARCH 280 specialty carbon black is suitable for use in printing inks, plastics and a variety of other applications including concrete and cement and general dispersions.
Printing inks: MONARCH 280 specialty carbon black is a high structure general purpose product that is broadly applicable in a variety of inks. It is particularly suitable for lithographic and gravure printing where a matte finish is required. This specialty carbon black offers very blue undertone and excellent dispersability.
Plastics: MONARCH 280 specialty carbon black is an effective opacifying agent for extruded films and is also widely used in UV applications such as utility pipe and agricultural film. In addition, it delivers good jetness and bluetone in a variety of general-purpose molded plastics parts.
Coatings: MONARCH 280 specialty carbon black is suitable for underbody/underhood automotive coatings as well as general industrial coatings where high jetness is not required. It is also suitable for use as a tinting black.
Other applications: This product is also used in concrete and cement, general dispersions and paper applications. MONARCH 280 specialty carbon black offers ease of dispersion and delivers good color, UV, and tinting performance. Its high structure, combined with low surface area, makes it one of the easiest to disperse Cabot specialty carbon blacks. However, the quality of the dispersion is affected by equipment choice and formulation. A product with similar morphology, BLACK PEARLS® 280 specialty carbon black, is available in an easier to handle pelleted form.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 g/cc0.00462 lb/in³ASTM D-1513
Particle Mesh Size 325 Mesh325 Mesh<50 ppm residue; ASTM D-1514
Ash 0.60 %0.60 %ASTM D-1506
 
Processing PropertiesMetricEnglishComments
Moisture Content 1.0 %1.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption45 mg/gCTM 23.4, Devolatilized
OAN119 cc/100gASTM D-2414
Product Formpowder
Tint0.6ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT161 / 315896

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.