Reinforced with 30 % of special GF and least anisotropy grade, meeting UL 94 V-2. Applications: Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecision machinery components that need dimensional accuracy, particularly least anisotropyComponents that need paint finish.Information provided by Teijin Chemicals Ltd. |