MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huntsman IROGRAN® A 85 H 4827 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range and offers a specially designed, flexible material with a broad processing window.

Performance Features:

  • High wear resistance
  • Medium crystallinity
  • Abrasion resistance
  • Flex resistance
  • Phthalate free TPU
Applications:
  • General Injection molding parts
  • Screens
  • Wheels and rollers
  • Shoe soles

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Injection molded parts; ASTM D792
Melt Index of Compound 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686Injection molded parts; ASTM D2240
Hardness, Shore D 3737Injection molded parts; ASTM D2240
Tensile Strength at Break 50.0 MPa7250 psiInjection molded parts; DIN 53504
Elongation at Break 600 %600 %Injection molded parts; DIN 53504
100% Modulus 6.00 MPa
@Strain 100 %
870 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 14.0 MPa
@Strain 300 %
2030 psi
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 85.0 kN/m485 pliInjection molded parts; DIN 53515
Abrasion 2020mm3, Injection molded; DIN 53516
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 185 - 195 °C365 - 383 °FInjection
Zone 1 87.8 - 93.3 °C190 - 200 °F
Zone 2 90.6 - 96.1 °C195 - 205 °F
Zone 3 93.3 - 98.9 °C200 - 210 °F
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding
Top Polymer Topolymer® 3200 TPE
Polyplastics TOPAS® Elastomer E-140 Cyclic Olefin Copolymer (COC)
Dow Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane

PHUQ097 / 159470

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.