Manufactured with a cotton fabric and phenolic resin, NP310E is easy to machine and possesses lower moisture absorption and enhanced electrical properties. NP310E meets or exceeds the requirements of MIL-I-24768/14.Information provided by Norplex-Micarta |
Cotton, Phenolic, Micarta, NEMA CE, MIL-I-24768/14-FBG, ASTM D709 Type II Grade CE |