MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Avient Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds to Polypropylene - ETO sterilizable and Autoclavable

Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Versaflex™ HC 2110-57B has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 0.5 to 2.5 in/sec Hold Time (Thick Part): 2 to 7 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D792
Viscosity 7.70e+6 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
Linear Mold Shrinkage, Flow 0.0070 - 0.012 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 59
@Temperature 23.0 °C
10 sec; ASTM D2240
Tensile Strength at Break 3.70 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 2.54 MPa
@Strain 100 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
 3.85 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 350 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 25.7 kN/mASTM D624
Compression Set 20 %
@Temperature 21.0 °C,
Time 79200 sec
ASTM D395B
 28 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 37 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 166 - 182 °C
Middle Barrel Temperature 193 - 216 °C
Front Barrel Temperature 204 - 227 °C
Nozzle Temperature 204 - 232 °C
Mold Temperature 12.8 - 32.2 °C
Screw Speed 80 - 120 rpm
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Agency RatingsISO 10993 Part 4
 ISO 10993 Part 5
AppearanceBlack
FeaturesGood Sterilizability
 Low Compression Set
 Low Friction
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesGaskets
 Medical/Healthcare Applications
 Overmolding
 Plugs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Avient Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT222 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT226 Thermoplastic Elastomer (TPE)

PH0POL1084 / 145653

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.