MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® BU50I PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU50I makes it ideal for applications in which the weld line impact strength at low temperatures is critical.

Applications: Automotive components, small engines, power tool parts and casings, cold weather and high impact supports gear, such as snowboards, ski components, helmets and hockey masks.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
Moisture Absorption at Equilibrium 2.1 %50% RH; ASTM D570
 7.3 %Saturation; ASTM D570
Linear Mold Shrinkage 0.04572 cm/cm1/8" bar
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 300 °C
Mold Temperature 60.0 - 85.0 °C
Dry Time 2 - 4 hour
Moisture Content <= 0.15 %
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® BU50I PA6 (Dry)
BASF Ultramid® BU50I BK 106 PA6 (Conditioned)
BASF Ultramid® BU50I BK 106 PA6 (Dry)
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Dry
BASF Capron® BU50I Ultratough Nylon 6 (Dry)

PBASG0440 / 132073

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.