MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Shanghai Potomer Trioctyl trimellitate
Categories: Other Engineering Material

Material Notes: Properties: it is light yellow ropy oily liquid, freezing point: -46 Degree Celsius, b.p. 260 Degree Celsius (0.15Kpa), ignition point 290 Degree Celsius, viscosity 210mPa.s(25 Degree Celsius), refractive index 1.485(25 Degree Celsius); soluble in most organic solvents.

Use: Trioctyl trimellitate(TOTM) is a fire-proof and lasting primary plasticizer, with the good points of polyester plasticizer and monomer plasticizer; suitable for PVC, cellulose nitrate, ethyl cellulose and poly(methyl methacrylate) etc.; its electrical property is pretty good and mainly used in the fire-proof electrical wires and cables of 105 Degree Celsius Level and other fire-proof and lasting panels, sheet materials, sealing gaskets and so on.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity <= 0.987 g/cc
Bulk Density 0.997 g/cc
Molecular Weight 547 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.30[mgKOH/g]
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 5.00e+11 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 240 °Copen cup
 
Descriptive Properties
Color/Appearance<150 Pt-CoLuster
Content>98.5%Ester
Heating Loss<0.15%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM124 / 284570

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.