Ketoprix™ EKT33G2L and EKT33G3L resins are thermoplastic aliphatic polyketone compounds where the polyketone base polymer consists of perfectly alternating a-olefins and CO to give the 1,4-diketone polymer backbone structure. To this base resin, fiber reinforcement, additional thermal stabilizers and lubricants are added to achieve desired mechanical performance and to assist in injection molding. These compounded resins are formulated for Injection Molded parts where higher strength and stiffness are required. Ketoprix™ EKT23G3C2/3 compounds are typically used in E&E, Automotive and Industrial End Uses.Information provided by Esprix Technologies. |