MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 20-3004 LV Chemical Resistant Epoxy System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3004 LV & HV are two component chemical resistance epoxy systems. They were developed for potting, coating, and adhesive applications requiring superior chemical resistance. They exhibit outstanding bonds to a variety of substrates. 20-3004 LV is a low viscosity self leveling system. 20-3004 HV is a high viscosity non-sag version.

Features:

  • Excellent chemical resistance
  • Excellent water resistance
  • Excellent adhesion to metals & plastics
  • DOT noncorrosive

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccResin
 1.17 g/cc1.17 g/ccHardener
Viscosity 5000 cP5000 cPHardener
 9000 cP9000 cPResin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878
Tensile Strength 52.4 MPa7600 psi
Elongation at Break 3.2 %3.2 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.613.61
Dissipation Factor 0.0210.021
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 140 °C284 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 50.0 °C122 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 90.0 min
@Temperature 100 °C
90.0 min
@Temperature 212 °F
 
Descriptive Properties
ColorBlackResin
 GreyMixed
 WhiteHardener
Mix Ratio100:45by weight, (Resin:Hardener)
 2:1by volume, (Resin:Hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX023 / 316700

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.