MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systems.

    Applications
  • Complex, thin-wall ductwork
    • Motorsports
    • Aerospace
    • Unmanned air vehicles (UAV’s)
  • Housings and enclosures
  • Impellers
  • Connectors
  • Consumer sporting goods
  • Vehicle dashboards and grilles
  • Bumpers
  • Snap-fit designs
  • Living hinges
  • Functional prototypes that require end-use performance properties
  • Appropriate for low- to mid-volume rapid manufacturing

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D792
Water Absorption 0.48 %
@Time 86400 sec
ASTM D570
Water Absorption at Saturation 1.15 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 69ASTM D785
Hardness, Rockwell M 34ASTM D785
Hardness, Shore D 74ASTM D2240
Tensile Strength, Ultimate 48.0 MPaASTM D638
Tensile Strength, Yield 37.0 MPaASTM D638
Elongation at Break 47 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 1517 MPaASTM D638
Flexural Strength 26.0 MPaUltimate; ASTM D790
Flexural Yield Strength 42.0 MPaASTM D790
Flexural Modulus 1310 MPaASTM D790
Izod Impact, Notched 74.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 14.86 J/cm
@Temperature 23.0 °C
ASTM D256
Gardner Impact 11.8 JASTM D5420
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.30e+13 ohm-cmASTM D257
Surface Resistance 4.90e+12 ohmASTM D257
Dielectric Constant 4.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.5 kV/mmASTM D149
Dissipation Factor 0.050
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831
 342 µm/m-°C
@Temperature 85.0 - 145 °C
ASTM E831
Specific Heat Capacity 1.75 J/g-°CASTM E1269
Thermal Conductivity 0.510 W/m-KASTM E1225
Deflection Temperature at 0.46 MPa (66 psi) 188 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems DuraForm® PA Nylon for SLS® Systems
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
Overview of materials for Polypropylene, Molded
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems

PAPPR118 / 83497

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.