MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem 9930 ZINC OXIDE TRANSPARENT
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Zinc Oxide Transparent is an accelerator activator of extremely fine particle size, particularly suited for transparent rubber goods. It can be employed in natural and synthetic rubbers and also as an acid acceptor in polychloroprene adhesives where transparency is required. It is especially useful for rubber articles which must be practically free from heavy metal traces.

Applications: Zinc Oxide Transparent is easy to incorporate and has very good dispersion characteristics in rubber compounds. Due to its small particle size, it causes a powerful activation of the cure. Zinc Oxide Transparent raises compound viscosities and, at high levels of addition, increases thermal conductivity and has a stiffening effect, improving the dimensional stability of extrusions and open cured goods.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.50 g/cc3.50 g/cc
Particle Mesh Size 230 Mesh230 Mesh99% thru
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 26 - 28 %26 - 28 %
Sulfate, SO4 <= 0.30 %<= 0.30 %
 
Descriptive Properties
Appearancewhite powder
Content<0.1%Chloride
 <10 ppmManganese
 <20 ppmCadmium
 <20 ppmLead Oxide
 <5 ppmCopper
 70-74%Zinc Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH658 / 315576

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.