MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kazanorgsintez Proxanol 305, 50%
Categories: Fluid; Solvent

Material Notes: Production Method: Obtained by interaction of ethylene glycol first with propylene oxide and then with ethylene oxide over an alkaline catalyst.

Application: 50% Proxanol 305 is used as an effective and universal demulsifying agent of oil emulsions, in the textile industry as a low-foaming penetrating agent of the peroxide stoving and dyeing process, for the artificial fiber industry as a reducing die fouling agent, in the spinning process of bulk dyed viscose silk, and as modifiers for high-strength viscose cord production.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearanceAt 20°C: Transparent of muddy liquid of yellow color, free of impurities
Congelation Temperature-45
Mass Content (%)48-52Mass content of active material
Temperature Limits, Solution Blooming, 100g/l Aqueous Solution of NaCl; 50 g/l (°C)50-60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAZAN145 / 127464

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.