MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF 2,4-Ethylmethylimidazole S
Categories: Fluid

Material Notes: Formula: C6H10O2

CAS: 931-36-2

Description: 2,4-Ethylmethylimidazole S is a colorless to yellowish liquid with an amine-like odor.

Synonyms: EMI, 2-Ethyl-4-methylimidazole, 4-Methyl-2-ethylimidazole, 2-Ethyl-4-methyl-1H-imidazole, 2-Ethyl-4(5)-methylimidazole

Applications: It is used as a Hardener for epoxy resins.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.0173 g/cc0.036752 lb/in³
Molecular Weight 110.2 g/mol110.2 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 36.0 - 42.0 °C96.8 - 108 °F
Boiling Point 270 - 276 °C518 - 529 °F
Flash Point 155 °C311 °F
Ignition Temperature 475 °C887 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.25 %<= 0.25 %DIN 51 777
 
Descriptive Properties
Assay83 - 86%
Color<10APHA, DIN EN 1557
Composition1-Methylimidazole1.0-2.0%
 2,4-Dimethyl-1H-imidazole1.0-4.0%
 4-Methylimidazole10-13%
 Active imidazoles95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
BASF AH-Salt
316 Stainless Steel, annealed bar
AISI 1045 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1045 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round

PBASG0945 / 132578

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.