MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aeos ePTFE Monofilament Suture Material
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Aeos® ePTFE Suture Monofilament (ASM) is made by extruding and expanding PTFE under controlled conditions during the manufacturing process. This process alters the physical properties of the product by creating microscopic pores in the structure of the material. The resulting product is imparted with unique physical properties such as flexibility and strength that make it ideal for suture applications. ePTFE has a long history of proven biological inertness in a variety of implant procedures including mitral valve and hernia repair, anastomosis, wound closure, and other vascular surgeries. Zeus ASM has the biocompatible history, maintains a high tensile strength in vivo, and is well-suited for stressful internal environments where absorbable sutures are not appropriate.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Monofilament Mean Diameter0.0080 in.Monofilament Size ASM 5
 0.0125 in.Monofilament Size ASM 4
 0.0155 in.Monofilament Size ASM 3
 0.0200 in.Monofilament Size ASM 2
 0.0240 in.Monofilament Size ASM 0
 0.0300 in.Monofilament Size ASM 1
Suture Knot-Pull Tensile Strength>1.10 lbfMonofilament Size ASM 5
 >1.10 lbfMonofilament Size ASM 4
 >1.10 lbfMonofilament Size ASM 3
 >1.10 lbfMonofilament Size ASM 2
 >1.10 lbfMonofilament Size ASM 0
 >1.10 lbfMonofilament Size ASM 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Iupilon® HL-3503 Polycarbonate
Vicryl Suture Material
Dexon Suture Material
Arkema Pebax® 4033 SP 01 Polyether Block Amide (PEBA)
Ethilon Suture Material

PZEUS960 / 192340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.