MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vycom CELTEC® Expanded Rigid foam PVC board
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface is a smooth matte finish that makes it ideal to paint or laminate to secondary substrates. Celtec also has good screw and staple retention which makes it ideal for stage prop design, cabinetry and other wood replacement projects. Sheets are tough, high-strength and lightweight, and can be ordered in a wide range of sizes, thicknesses and colors. Celtec sheets are free of lead, cadmium, barium and zinc. Celtec is recommended for industrial and commercial signage. It readily accepts virtually any form of graphic overlay (print, paint and photo mounting). Celtec is also easy to cut and shape, making it a strong choice for three-dimensional exhibits, displays and stage sets.

FEATURES AND BENEFITS

  • Lightweight- Celtec is easy to handle, easy to work with.
  • Low Flammability- Celtec meets UL94 5V, UL 1975 and has a flame spread of 20 according to ASTM E84.
  • Water resistant- Celtec has a closed cell structure and has extremely low water absorption values.
  • Surface- Celtecs smooth matte surface is ideal for graphics, printing and laminating.
  • Weatherability- Celtec is more color-fast than other foam PVC products.
  • Strength- Celtec has an excellent strength to weight ratio as shown in the screw and staple pull test data.
  • Thermal Conductivity- Celtec has excellent insulating characteristics.
  • Safety- Celtec contains no lead, cadmium or zinc.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.550 g/cc
@Thickness 10.0 - 25.0 mm
ASTM D792
 0.700 g/cc
@Thickness 1.00 - 6.00 mm
ASTM D792
Water Absorption 0.15 %
@Thickness 10.0 - 25.0 mm
ASTM D570
 0.30 %
@Thickness 1.00 - 6.00 mm
ASTM D570
 0.90 %
@Thickness 1.00 - 6.00 mm
ASTM D2842
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2256 psi
@Thickness 10.0 - 25.0 mm
ASTM D638
 3000 psi
@Thickness 1.00 - 6.00 mm
ASTM D638
Tensile Modulus 144000 psi
@Thickness 10.0 - 25.0 mm
ASTM D638
 232000 psi
@Thickness 1.00 - 6.00 mm
ASTM D638
Flexural Strength 3329 psi
@Thickness 10.0 - 25.0 mm
ASTM D790
Flexural Modulus 144200 psi
@Thickness 10.0 - 25.0 mm
ASTM D790
Izod Impact, Notched 0.530 ft-lb/in
@Thickness 1.00 - 6.00 mm
ASTM D256
Charpy Impact, Unnotched 4.50 ft-lb
@Thickness 10.0 - 25.0 mm
ASTM D256
 8.10 ft-lb
@Thickness 1.00 - 6.00 mm
ASTM D256
Gardner Impact 8.58 ft-lb
@Thickness 10.0 - 25.0 mm
ASTM D4228
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 11.2 kV/mm
@Thickness 1.00 - 6.00 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Thickness 10.0 - 25.0 mm,
Temperature 20.0 °C
ASTM D696
 40.0 µin/in-°F
@Thickness 1.00 - 6.00 mm,
Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.0840 W/m-K
@Thickness 1.00 - 6.00 mm
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 150 °F
@Thickness 10.0 - 25.0 mm
ASTM D648
 151 °F
@Thickness 1.00 - 6.00 mm
ASTM D648
Flammability, UL94 V-0
@Thickness 1.00 - 6.00 mm
5V
Flame Spread Index 20
@Thickness 10.0 - 25.0 mm
ASTM E84
 20
@Thickness 1.00 - 6.00 mm
ASTM E84
 
Descriptive Properties
Burning RateNo burn when flame removed
Foam FirePassed/ClassifiedUL 1975
Nail Hold, Lbf/in penetration35ASTM D1761
Oil Canning; (at 140°F) 10mm - 25mmPassedASTM D648
Screw Hold, Lbf/in penetration680ASTM D1761
Staple Hold, Lbf/in penetration180ASTM D1761

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
G-11 Fiberglass Epoxy Laminate Sheet
Overview of materials for PVC, Molded
Overview of materials for PVC, Sheet Grade
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber

PCPCV00 / 29072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.