MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM PR/721 Flame Retardant Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant polyolefinic compounds

FRAGOM PR/720: halogen-free flame-retardant polyolefinic thermoplastic compound with high values of temperature index and oxygen index, very easy to process and suitable for cable sheathing. The compound was developed to use in sheathing extrusion especially when the thickness is important (1,8-2,4 mm)

Certify: CEI 2011 M1, VDE 0207 HM2, BS 7655 LTS1-LTS3

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 21.6 kg,
Temperature 160 °C
IEC 60811
 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
IEC 60811
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 46ASTM D2240
Tensile Strength >= 13.0 MPaIEC 60811
 >= 13.65 MPa
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 60811
 >= 14.95 MPa
@Temperature 70.0 °C,
Time 14400 sec
Ageing in oil, SAE 20; IEC 60811
Elongation at Break 190 %IEC 60811
 163.4 %
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 60811
 209 %
@Temperature 70.0 °C,
Time 14400 sec
Ageing in oil, SAE 20; IEC 60811
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 80.0 °C
@Time 14400 sec
<35%, Penetration; IEC 60811
Oxygen Index 40 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 120 °C
Zone 2 135 °C
Zone 3 150 °C
Zone 4 160 °C
Die Temperature 175 °C
Head Temperature 165 °C
Dry Time 2.00 hour
@Temperature 80.0 °C
 3.00 hour
@Temperature 90.0 °C
 
Descriptive Properties
Halogen Content< 0,1%IEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS103 / 294187

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.