MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Arquad 2C-75 EMEIA Dicocoalkyldimethyl ammonium chloride
Categories: Other Engineering Material

Material Notes: Arquad 2C-75 is a quaternary ammonium compound.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.860 g/cc
@Temperature 60.0 °C
0.0311 lb/in³
@Temperature 140 °F
 0.880 g/cc
@Temperature 20.0 °C
0.0318 lb/in³
@Temperature 68.0 °F
pH 6.0 - 9.06.0 - 9.05% in 50/50 2-Propanol/water
Viscosity  50 cP
@Temperature 60.0 °C
50 cP
@Temperature 140 °F
 120 cP
@Temperature 25.0 °C
120 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -20.0 - -10.0 °C-4.00 - 14.0 °F
Flash Point 28.0 °C82.4 °FDIN 51755
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 5.0<= 5.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 10 %10 %
 
Descriptive Properties
AppearanceYellow liquid
Content= 0.5 %Salt
 = 2%(Mw=397/433.5), Free Amine & Amine Salt
 74-77%(Mw=447.5), Active content
Content(%)152-Propanol
HLB17Davies
Odor2-propanol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY296 / 285819

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.