Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production. Dyneon offers a family of PTFE fine powder paste extrusion resins. These products are well suited for a variety of applications, including tubing, hose, pipe liners, tapes, wire and cable, diaphragms and textile/fiber. Available grades are designed to balance process properties such as reduction ratio, and performance properties, such as tensile strength, shrinkage, flex life and permeations. Data provided by Dyneon. |