MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Selenis AKOLYT KB 311 Copolyester for Film Extrusion
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Selenis Akolyt KB 311 copolyester has been specifically developed for the extrusion of technical films for graphic arts in general. Films made with Selenis Akolyt KB 311 allow excellent decorative capability, permitting unlimited design freedom and full personalization of the final application. The exceptional clarity of films produced with Selenis Akolyt KB 311 allow reverse printing technique, enhancing printing optics while maximizing artwork protection. Elongation of films produced with Selenis Akolyt KB 311 permit thermoformed deep drawing, at the same time as its relatively low Tg grants energy cost savings while guaranteeing perfect adhesion to itself. Proven chemical resistance against common household detergents makes Selenis Akolyt KB 311 the perfect choice for films that will resist everyday weathering.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.730 g/cc0.0264 lb/in³
Density >= 1.29 g/cc>= 0.0466 lb/in³ASTM D792
Water Absorption <= 0.12 %<= 0.12 %ASTM D570
Moisture Absorption at Equilibrium <= 0.30 %<= 0.30 %
Viscosity Test 78 - 82 cm³/g0.78 - 0.82 dl/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0<= 1.0b*; ASTM D6290
 >= 64>= 64L*; ASTM D6290
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 19.0 MPa2760 psi(sb); ISO 527-2
Tensile Strength 53.0 MPa7690 psi(σm); ISO 527 -1/- 2
Tensile Strength, Yield 53.0 MPa7690 psi(σy); ISO 527 -1/- 2
Elongation at Break 31 %31 %Nominal, (εtb); ISO 527 -1/- 2
Elongation at Yield 4.0 %4.0 %(εm); ISO 527 -1/- 2
 4.0 %4.0 %(εy); ISO 527 -1/- 2
Tensile Modulus 3.00 GPa435 ksiISO 527-2
Flexural Strength 71.0 MPa10300 psiISO 178
Flexural Modulus 2.04 GPa296 ksiISO 178
Izod Impact, Notched (ISO)  3.90 kJ/m²
@Temperature -30.0 °C
1.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 4.40 kJ/m²
@Temperature 0.000 °C
2.09 ft-lb/in²
@Temperature 32.0 °F
ISO 180
 4.50 kJ/m²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180
Izod Impact, Unnotched (ISO)  125 kJ/m²
@Temperature -30.0 °C
59.5 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FISO 75-2
Vicat Softening Point 78.0 °C172 °FISO 306
Glass Transition Temp, Tg 80.0 °C176 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 250 °C356 - 482 °F
Drying Temperature <= 70.0 °C<= 158 °Fto avoid chips sticking together in dryer hopper
 60.0 - 65.0 °C
@Time 18000 - 21600 sec
140 - 149 °F
@Time 5.00 - 6.00 hour
Moisture Content <= 0.0040 %<= 0.0040 %dried
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Deflection at Flexural Strength8.6 mm
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSELE905 / 243403

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.