MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Vulkanox® SKF Rubber Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Aging processes, which are caused by oxygen or heat, change the properties of the vulcanizates. Rubbers generally are subject to such changes that occur in the course of time and can lead to partial or complete destruction. Possible consequences are depolymerization, fatigue, brittleness, cracks and even disintegration. The resistance of a rubber article to oxygen, ozone and other reactive substances is determined mainly by the elastomer on which the compound is based and by the chemicals that are added to retard the destructive processes. Unsaturated groups in the rubber molecule are the reason for the rubber's sensitivity to oxygen, which increases with temperature. If catalysts of oxidation (known as rubber poisons) are present, aging is rapid. The results are hardening and embrittlement, crazing effects and fatigue. Ozone or dynamic stress (fatigue) lead to cracking on the surface of the rubber article. Antidegradants such as Vulkanox® are chemicals which protect the vulcanizates against damaging external influences. Depending on the chemical structure, they act against one or more of the aging processes mentioned. None of the antidegradants is universally effective, each has a definite spectrum of activity and characteristic effectiveness, and a definite propensity to discolor the goods if they are exposed to light. Staining antidegradants are generally more effective than nonstaining ones.

Key Properties:

  • protection against oxidation, ozone, heat and rubber poisons
  • protection against dynamic stress

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Volatiles <= 0.50 %
@Temperature 105 °C,
Time 3600 sec
<= 0.50 %
@Temperature 221 °F,
Time 1.00 hour
10g; DIN ISO 787/2
Ash <= 0.10 %<= 0.10 %ASTM D 4574
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 105 °C>= 221 °FASTM D1519A
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearancewhite to cream-colored powder
Specifications<0.5%Sieve residue (0.063 mm), ASTM D4572

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY9171 / 209562

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.