MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Pibifor® K2 E9/2A PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Elastomer modified PBT, Good Impact Resistance even at Low Temperature

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D1505
Water Absorption 0.40 %ASTM D570
Moisture Absorption at Equilibrium 0.20 %
Linear Mold Shrinkage 0.016 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 2400 MPaASTM D638
Flexural Modulus 1800 MPaASTM D790
Izod Impact, Notched 200 J/mASTM D256
Charpy Impact, Notched 25.0 kJ/m²ISO 179 1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 - 260 °CCylinder Temperature
Mold Temperature 50.0 - 90.0 °C
Drying Temperature 110 °C
@Time 10800 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PEKK, Unreinforced
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Kraton® FG1901 + PET blend (20/80)
Klinger Thermoseal Milam Mica PSS 130 Laminate
Goodfellow CVD Graphene Film on PET

PSOFS922 / 162386

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.