MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2020211D3 Electrode Ink  (discontinued **)
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Electrode Ink C2020211D3 is a Silver Palladium (70/30) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.

The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is designed for printing on PVB tape.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 49 - 51 %49 - 51 %
Particle Size 1.0 µm1.0 µmMain Break; Fineness of Grind
 4.0 µm4.0 µm3rd Streak; Fineness of Grind
Viscosity 6900 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
6900 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C68.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  <= 1.98 min
@Temperature 150 °C
<= 0.0330 hour
@Temperature 302 °F
touch dry
 <= 4.02 min
@Temperature 75.0 °C
<= 0.0670 hour
@Temperature 167 °F
touch dry
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Coverage cm2/g245230 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGEM085 / 75938

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.