MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plenco 50335 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.

Information supplied by Plenco


Plenco discontinued their PET product line in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³ASTM D792
Water Absorption 0.070 %0.070 %ASTM D570
Linear Mold Shrinkage 0.0024 cm/cm0.0024 in/inATM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 123.9 MPa17970 psiASTM D638
Elongation at Break 1.99 %1.99 %ASTM D638
Flexural Yield Strength 187.2 MPa27150 psiASTM D790
Flexural Modulus 8.74 GPa1270 ksiASTM D790
Compressive Yield Strength 170.7 MPa24760 psiASTM D695
Izod Impact, Notched 0.540 J/cm1.01 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 9.14e+15 ohm-cm9.14e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.4 kV/mm493 kV/inShort Time; ASTM D149
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 200 V200 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FASTM D648
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Plenco 50240 PET, Pellet, Injection Molded, Natural Color
Pearl Engineering PEPLPET B-105C PET Bottle Grade
Pearl Engineering PEPLPET B-103C PET Bottle Grade

PLEM73 / 50761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.