MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Master Bond MB297Med-3 Ethyl Cyanoacrylate
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Key Features:
  • One component, no mix system
  • Meets USP Class VI specifications
  • Fast setting
  • Rapid fixture time
Product Description: Master Bond MB297Med-3 is a single component ethyl cyanoacrylate type adhesive. This high strength, rapid curing system is used primarily for medical device assembly. MB297Med-3 is a very low viscosity (10-20 cps) cyanoacrylate. This kind of system, which is commonly referred to as an instant adhesive or super glue, cures very rapidly with the rate of cure dependent upon the humidity—the higher it is, the faster the cure. Because curing is normally so fast, minimal contact pressure is usually sufficient for bonding. It must be emphasized that this high strength system requires no heating or mixing. It typically sets up within 5 to 35-40 seconds depending upon the humidity and the substrates. The bond strength is exceptionally high in the shear mode. MB297Med-3 bonds well to a variety of substrates especially metals, plastics and rubbers. The service temperature range for this system is -60°F to +250°F. Most importantly, MB297Med-3 meets USP Class VI specifications for biocompatibility. MB297Med-3 can be used in a wide array of different medical applications ranging from repair to high speed production. It has first rate resistance to EtO and gamma sterilization processes. Although many of the applications for MB297Med-3 involve disposable type medical devices, it also can be utilized with reusable ones depending upon the service conditions.

Product Advantages:

  • Rapid curing at room temperature; usually sets up within 35-40 seconds
  • No heating or mixing
  • Contact pressure usually sufficient for fixturing
  • Bonds well to a wide variety of substrates
  • Excellent resistance to EtO and gamma sterilization
  • Passes USP Class VI testing
  • Well suited for disposable and reusable medical devices

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 10 - 20 cP10 - 20 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
Tensile Strength 27.6 - 31.0 MPa4000 - 4500 psi
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %
Tensile Modulus 1.38 - 1.72 GPa200 - 250 ksi
Adhesive Bond Strength 1.45 MPa210 psiButyl-Butyl, Tensile lap; Substrate Failure
 2.07 MPa300 psiSteel-Natural Rubber, Tensile lap; Substrate Failure
 2.41 MPa350 psiSteel-Butyl, Tensile lap; Substrate Failure
 2.90 MPa420 psiNatural Rubber-Natural Rubber, Tensile lap; Substrate Failure
 3.03 MPa440 psiSBR-SBR, Tensile lap; Substrate Failure
 3.24 MPa470 psiNeoprene-Steel, Tensile lap
 3.52 MPa510 psiNBR-NBR, Tensile lap; Substrate Failure
 3.52 MPa510 psiNitrile-Nitrile, Tensile lap; Substrate Failure
 3.59 MPa520 psiNeoprene-Neoprene, Tensile lap; Substrate Failure
 3.93 MPa570 psiPolystyrene-Polystyrene, Tensile lap; Substrate Failure
 5.86 MPa850 psiDelrin-Delrin, Tensile lap
 6.07 MPa880 psiNylon-Nylon, Tensile lap
 6.34 MPa920 psiNylon-Bakelite, Tensile lap
 6.55 MPa950 psiNBR-Aluminum, Tensile lap
 7.24 MPa1050 psiAluminum-Aluminum, Tensile lap
 7.24 MPa1050 psiChromium-Chromium, Tensile lap
 8.41 MPa1220 psiPhenolic-Phenolic, Tensile lap
 8.48 MPa1230 psiABS-ABS, Tensile lap; Substrate Failure
 9.72 MPa1410 psiNylon-Copper, Tensile lap; Substrate Failure
 10.9 MPa1580 psiAluminum-Stainless Steel, Tensile lap
 11.4 MPa1650 psiSteel-Stainless Steel, Tensile lap
 14.1 MPa2050 psiSteel-PVC (rigid), Tensile lap; Substrate Failure
 14.38 MPa2085 psiPolyester-Polyester, Tensile lap
 15.9 MPa2300 psiCopper-Copper, Tensile lap
 15.9 MPa2310 psiSteel-Aluminum, Tensile lap
 16.1 MPa2330 psiStainless-Stainless, Tensile lap
 16.1 MPa2340 psiSteel-Steel, Tensile lap
 16.2 MPa2350 psiBrass-Brass, Tensile lap
 18.4 MPa2670 psiPVC(rigid)-PVC(rigid), Tensile lap; Substrate Failure
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 3.6
@Frequency 1000 Hz
3.6
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 75.0 µm/m-°C38.9 - 41.7 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Softening Point 138 - 143 °C280 - 290 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0830 - 0.670 min0.00138 - 0.0112 hourset up time, substrate dependent
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
in original, unopened containers
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
ColorColorless, transparent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MB297Med Ethyl Cyanoacrylate Biocompatible Adhesive System
Master Bond MB297Med-1 Ethyl Cyanoacrylate
Master Bond MB297Med-2 Ethyl Cyanoacrylate
Americhem Engineered Compounds ColorRx™ PE2-0202ARX Biocompatible, Antimicrobial HDPE
Americhem Engineered Compounds ColorRx™ PE2-0201A Antimicrobial HDPE

PMASTM926 / 185519

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.