MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Thermoset™ EX-5640 Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD Thermoset EX-5640 adhesive is a semi-thixotropic, two-component structural adhesive system used to bond various materials together for electronic applications.

Features: provides excellent wetting to most metal, plastic and ceramic substrate surfaces without dripping/slumping off.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 - 1.09 g/cc1.06 - 1.09 g/cccurative
 1.00 - 1.20 g/cc1.00 - 1.20 g/ccresin
Viscosity  5000 - 7500 cP
@Temperature 25.0 °C
5000 - 7500 cP
@Temperature 77.0 °F
Spindle 6, 50 rpm
 17000 - 20000 cP
@Temperature 25.0 °C
17000 - 20000 cP
@Temperature 77.0 °F
Spindle 7, 50 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 90
@Temperature 24.0 °C
80 - 90
@Temperature 75.2 °F
cured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 ohm-cm
@Temperature 77.0 °F
cured
Dielectric Constant 4.2
@Frequency 100000 Hz
4.2
@Frequency 100000 Hz
Dielectric Strength 15.7 - 19.7 kV/mm400 - 500 kV/in
Dissipation Factor 0.035
@Frequency 100000 Hz
0.035
@Frequency 100000 Hz
Arc Resistance 88 sec88 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 51.0 µm/m-°C28.3 µin/in-°Fby TMA, cured
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°Fcured
 
Processing PropertiesMetricEnglishComments
Gel Time  10.0 min
@Temperature 65.0 °C
10.0 min
@Temperature 149 °F
 20.0 - 45.0 min
@Temperature 25.0 °C
20.0 - 45.0 min
@Temperature 77.0 °F
Shelf Life 6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
from date of manufacture in original, unopened container
 
Descriptive Properties
AppearanceOff-white LiquidResin
 Red LiquidCurative
 Red LiquidMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin
Henkel Hysol EA 9150 Composite Resin
Glyptal 74004 Epoxy Enamel
Emerald Performance Materials EPALLOY® 9000 Modified Bisphenol A Epoxy Resin
Emerald Performance Materials EPALLOY® 8220 Bisphenol F Epoxy Resin

PLORD9160 / 232548

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.