MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machining and clearing away of the rolled surface on both sides.

Information provided by ALIMEX GmbH

Solution heat-treated, stress-relieved by stretching a controlled amount and then artificially aged. / Solution heat treated, stress relieved by compressing to produce a permanent set of 1% to 5% and then artificially aged.

Key Words: EN AW-7975 (AlZn5,5MgCu)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.100 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105 - 160
Tensile Strength, Ultimate 360 - 540 MPaRm
Tensile Strength, Yield 260 - 470 MPa
@Strain 0.2 %
Elongation at Break <= 6.0 %
Modulus of Elasticity 70.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000435 - 0.00000526 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 902.2 - 1110 BTU-in/hr-ft²-°F
 
Descriptive Properties
Machinability Good
Protective AnodizingSuitable, not decorative
Welding Properties (WIG, MIG)Less Suitable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Alclad Aluminum 7075-T6, T651
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
Aluminum 7075-O

NALIMEX06 / 14761

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.