MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake Plastics Halar® 901 ECTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impact strength, and a broad service use temperature. This polymer offers extremely low permeability to liquids, gases, and vapors.

Halar® is a trade name of Solvay Solexis, Inc. Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D792
Water Absorption <= 0.10 %ASTM D570; 24 hrs.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4300 psiASTM D638
Elongation at Break 250 %ASTM D638
Tensile Modulus 240000 psiASTM D638
Flexural Yield Strength 3800 psiASTM D790
Flexural Modulus 245000 psiASTM D790
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 350 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 56.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Melting Point 465 °FASTM D4591
Maximum Service Temperature, Air 300 °FContinuous Use
Deflection Temperature at 1.8 MPa (264 psi) 145 °FASTM D648
Flammability, UL94 V-0
Oxygen Index 56 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
VICTREX™ PEEK 450G™ General Purpose
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Syensqo (Solvay Specialty Polymers) Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Syensqo (Solvay Specialty Polymers) Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)

PWEST143 / 72762

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.