Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.38 g/cc @Thickness 12.7 mm | 1.38 g/cc @Thickness 0.500 in |
Moisture Absorption | 1.30 % @Thickness 1.57 mm | 1.30 % @Thickness 0.0620 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell M | 101 @Thickness 6.35 mm | 101 @Thickness 0.250 in |
Tensile Strength | 82.7 MPa @Thickness 3.17 mm | 12000 psi @Thickness 0.125 in |
| 96.5 MPa @Thickness 3.17 mm | 14000 psi @Thickness 0.125 in |
Flexural Strength | 103 MPa @Thickness 1.57 mm | 15000 psi @Thickness 0.0620 in |
| 138 MPa @Thickness 1.57 mm | 20000 psi @Thickness 0.0620 in |
Flexural Modulus | 7.24 GPa @Thickness 1.57 mm | 1050 ksi @Thickness 0.0620 in |
| 8.96 GPa @Thickness 1.57 mm | 1300 ksi @Thickness 0.0620 in |
Compressive Strength | 207 MPa @Thickness 12.7 mm | 30000 psi @Thickness 0.500 in |
Shear Strength | 88.3 MPa @Thickness 1.57 mm | 12800 psi @Thickness 0.0620 in |
Izod Impact, Unnotched | 0.240 J/cm @Thickness 12.7 mm | 0.450 ft-lb/in @Thickness 0.500 in |
| 0.294 J/cm @Thickness 12.7 mm | 0.550 ft-lb/in @Thickness 0.500 in |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Constant | 6.1 @Thickness 1.57 mm, Frequency 1e+6 Hz | 6.1 @Thickness 0.0620 in, Frequency 1e+6 Hz |
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm | 600 kV/in @Thickness 0.0620 in |
| 27.6 kV/mm @Thickness 1.57 mm | 700 kV/in @Thickness 0.0620 in |
Dielectric Breakdown | 10000 V @Thickness 1.57 mm | 10000 V @Thickness 0.0620 in |
| 40000 V @Thickness 1.57 mm | 40000 V @Thickness 0.0620 in |
Dissipation Factor | 0.050 @Thickness 1.57 mm, Frequency 1e+6 Hz | 0.050 @Thickness 0.0620 in, Frequency 1e+6 Hz |
Arc Resistance | 110 sec @Thickness 3.17 mm | 110 sec @Thickness 0.125 in |
Comparative Tracking Index | 200 V @Thickness 3.17 mm | 200 V @Thickness 0.125 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Thickness 3.17 mm | 8.33 µin/in-°F @Thickness 0.125 in |
CTE, linear, Transverse to Flow | 19.0 µm/m-°C @Thickness 3.17 mm | 10.6 µin/in-°F @Thickness 0.125 in |
UL RTI, Electrical | 130 °C | 266 °F |
UL RTI, Mechanical with Impact | 130 °C | 266 °F |
Flammability, UL94 | HB @Thickness 1.57 mm | HB @Thickness 0.0620 in |
|
Descriptive Properties |
---|
Bonding Strength | 1000 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.