MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Eastotac™ C-100R Resin
Categories: Polymer

Material Notes: Product Description: Eastotac™ C-100R Resin is a tackifier resin with a ring and ball softening point of 100°C and a molten Gardner color of 4.

Application/Uses:

  • Asphalt Modification
  • Assembly
  • Automotive
  • Bookbinding
  • Building and Construction
  • Caulks and Sealants
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
  • Wire and Cable
Key Attributes:
  • Broad compatibility with numerous elastomers, polymers, and other tackifying resins
  • Consistent quality
  • Excellent heat stability
  • Light color
  • Low odor

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Brookfield Viscosity 150 cP
@Temperature 190 °C
150 cP
@Temperature 374 °F
Molecular Weight 550 g/mol550 g/molMn
 1100 g/mol1100 g/molMw. Mw/Mn ratio = 2
 2100 g/mol2100 g/molMz
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 100 °C212 °FASTM E 28
 
Optical PropertiesMetricEnglishComments
Yellow Index 11 %11 %1 cm cell; ASTM E 313
Gardner Color Number <= 1.5<= 1.5ASTM D6166
 4.04.0Molten
 
Descriptive Properties
Cloud Point<-50°COMSCP
 56°CDACP
 78°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5298 / 222492

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.