MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTANT® PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Product characteristics:
  • Good dimensional stability
  • Low moisture absorption
  • High stiffness
Product applications:
  • Electrical industry
  • Safety engineering
  • Automotive industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 %0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282DIN EN ISO 868
Tensile Strength, Yield 65.0 MPa9430 psiDIN EN ISO 527
Elongation at Break 80 %80 %DIN EN ISO 527
Modulus of Elasticity 2.30 GPa334 ksiDIN EN ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohmDIN EN 62631-3-2
Dielectric Constant 3.03.0IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 275 V275 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FDIN 53752
Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°FDIN 52612
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 115 °C239 °Flong term
 140 °C284 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FDIN EN ISO 75
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S KR 2864C Colored ASA+PC
Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber
Ter Hell Plastic Terez® PC 9007 UV Polycarbonate
Röhm CyRex® 300 Acrylic-Polycarbonate Alloy
Röchling SUSTANT® PC GF 20

PROCH9314 / 233016

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.