MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Regal® 32 R&O
Categories: Fluid; Lubricant

Material Notes: Texaco Regal R&O oils deliver value through:
  • Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high temperature conditions for longer service life.
  • Saves on maintenance and downtime — Highly refined base stocks and multi-component oxidation inhibitor system resist the formation of harmful sludge and varnish deposits. The special rust inhibitor protects components against corrosion.
  • Trouble-free operation — Excellent water separability of the highly refined base stocks and special inhibitor system ensure rapid settling of harmful water accumulated from steam condensate. The nonsilicone foam inhibitor allows rapid release of entrained air while minimizing foam formation to enable reliable operation of sensitive hydraulic control devices.
  • Saves on inventory — Good quality rust and oxidation inhibited formulation has multipurpose capability in a wide range of industrial applications for which this type of product is recommended, simplifying oil inventories and reducing the possibility of using the wrong lubricant.

Texaco Regal R&O oils are inhibited turbine oils formulated from highly refined base stocks and rust, oxidation, and foam inhibitors.

Texaco Regal R&O oils are good quality lubricants for any application not requiring antiwear or extreme pressure protection.

The natural thermal and oxidation stability of these lubricants, due to their high level of refinement, has been further enhanced by their unique additive systems. The high thermal and oxidation stability also reduces the possibility of oxidation deposits or the generation of acidic material from oxidation.

Texaco Regal R&O oils are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.

They minimize entrained air which otherwise could result in low lubricant film strength between moving parts and pump cavitation.

Texaco Regal R&O 32 through 150 are recommended for use in electric motor bearings, air compressors, gears, hydroelectric turbines, steam turbines, combustion turbine generators (gas), marine turbines, and hydraulic systems (except heavy duty systems).

These products can also be used as a general purpose machine oil for shop use. Texaco Regal R&O 46 - 460 meet the requirements of ANSI/AGMA 9005-E02 for gear lubrication as rust and oxidation inhibited gear oils.

Do not use Texaco Regal R&O 32, 46, or 68 in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Do not use in breathing air apparatus or medical equipment.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220700; MSDS Number: 8608

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.9 °ASTM D287
Viscosity Measurement 100Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 157 SUSASTM D445
Saybolt Viscosity at 210°F 43.7 SUSASTM D445
Kinematic Viscosity at 40°C (104°F) 30.4 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.2 cStASTM D445
Oxidative Stability >= 16.7 hourto 25 psi drop; ASTM D2272
 >= 7000 hourHours to 2 mg KOH/g acid number; ASTM D943
 
Thermal PropertiesOriginal ValueComments
Pour Point -33.0 °CASTM D97
Flash Point 222 °CASTM D92
 
Descriptive Properties
Rust PreventionPass24 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ TC-208 Thermally Conductive Grease
ExxonMobil Mobil Rarus 824
ExxonMobil Mobil Aero HFA
Dow HIGH VACUUM GREASE
ChevronTexaco TEGRA® Synthetic Barrier Fluid

WTEXA160 / 77039

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.