MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici RADILON® S HSX88 100 NT Nylon 6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: PA6 injection molding grade. Toughened. Natural color. Suitable for parts requiring improved impact resistance

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: High impact or impact modified

Industries: Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Water Absorption 8.8 %
@Thickness 2.00 mm
8.8 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
2.60 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress  10.0 MPa
@Strain 1 %
1450 psi
@Strain 1 %
 20.0 MPa
@Strain 3 %
2900 psi
@Strain 3 %
 37.0 MPa
@Strain 20 %
5370 psi
@Strain 20 %
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ISO 527-2/1A
Elongation at Break >= 100 %>= 100 %Nominal, 50 mm/min; ISO 527-2/1A
Tensile Modulus 0.900 GPa131 ksi1mm/min; ISO 527-2/1A
Flexural Strength 30.0 MPa4350 psi2mm/min; ISO 178
Flexural Modulus 0.800 GPa116 ksi2mm/min; ISO 178
Secant Modulus  0.200 GPa
@Strain 19 %
29.0 ksi
@Strain 19 %
 0.600 GPa
@Strain 5.0 %
87.0 ksi
@Strain 5.0 %
 1.00 GPa
@Strain 0.0 %
145 ksi
@Strain 0.0 %
Charpy Impact, Notched 6.50 J/cm²30.9 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohm500V; IEC 60093
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI120 / 313621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.