MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Haynes Multimet® Alloy, GTAW, Sheet/Plate
Categories: Metal; Superalloy; Iron Base

Material Notes: Short time tensile data for gas tungsten-arc weldments, as-welded.

Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductility, and is readily fabricated. Current applications include aircraft, including tailpipes and tailcones, afterburner parts, exhaust manifolds, combustion chambers, turbine blades, buckets and nozzles. Excellent service for high temperature bolts.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AMS 5794, UNS R30155, AMS 5532, AMS 5768, AMS 5769, AMS 5795
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 105900 psi
@Thickness 9.52 mm
 108200 psi
@Thickness 3.17 mm
 111400 psi
@Thickness 6.35 mm
Tensile Strength, Yield 60400 psi
@Thickness 9.52 mm
 60500 psi
@Thickness 3.17 mm
 65000 psi
@Thickness 6.35 mm
Elongation at Break 19 %
@Thickness 9.52 mm
in 50.8 mm
 21 %
@Thickness 6.35 mm
in 50.8 mm
 22 %
@Thickness 3.17 mm
in 50.8 mm
Poissons Ratio 0.298RT
 0.315
@Temperature 426 °C
 0.319
@Temperature -78.0 °C
 0.325
@Temperature 650 °C
 0.339
@Temperature 816 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000930 ohm-cm
@Temperature 22.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.3 µm/m-°C
@Temperature 23.0 - 300 °C
 15.6 µm/m-°C
@Temperature 23.0 - 400 °C
 16.0 µm/m-°C
@Temperature 23.0 - 500 °C
 16.7 µm/m-°C
@Temperature 23.0 - 600 °C
 17.2 µm/m-°C
@Temperature 23.0 - 700 °C
 17.5 µm/m-°C
@Temperature 23.0 - 800 °C
 17.8 µm/m-°C
@Temperature 23.0 - 900 °C
 17.8 µm/m-°C
@Temperature 23.0 - 1000 °C
 18.4 µm/m-°C
@Temperature 23.0 - 1100 °C
Specific Heat Capacity 0.435 J/g-°C
@Temperature >=100 °C
Thermal Conductivity 15.9 W/m-K
@Temperature 300 °C
 17.3 W/m-K
@Temperature 400 °C
 18.6 W/m-K
@Temperature 500 °C
 20.0 W/m-K
@Temperature 600 °C
 20.0 W/m-K
@Temperature 200 °C
Melting Point 1288 - 1354 °C
Solidus 1288 °C
Liquidus 1354 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.88
@Temperature 1090 °C
Oxidized
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.080 - 0.16 %
Cb + Ta 0.75 - 1.25 %
Chromium, Cr 20 - 22.5 %
Cobalt, Co 18.5 - 21 %
Iron, Fe 33 %As remainder
Manganese, Mn 1.0 - 2.0 %
Molybdenum, Mo 2.5 - 3.5 %
Nickel, Ni 19 - 21 %
Nitrogen, N 0.10 - 0.20 %
Silicon, Si <= 1.0 %
Tungsten, W 2.0 - 3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Crucible Steel 440B Chromium Steel
Copper nickel 30%, UNS C71500, O61 Temper 1 mm strip

NHAMCD / 16846

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.