MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick
Categories: Ceramic; Carbide

Material Notes: Silicon nitride-bonded silicon carbide brick has the following characteristics:
  • Max. service temperature 1580°C (2876°F)
  • For sidewall lining of aluminum reduction cells
  • High thermal conductivity
  • Low porosity
  • Low thermal expansion
  • Low gas permeability
  • Outstanding abrasion and erosion resistance
  • High modulus of rupture
  • Superior resistance to metal penetration and attack
  • Extremely high crushing strength
  • Excellent oxidation resistance and resistance to corrosion

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 165 lb/ft³EN 993-1 1995
Porosity 17 %Apparent; EN 993-1 1995
Permeability <= 0.050nPm, Permeability to gases; EN 993-4 1995
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0440 GPaEN 993-6: 1995
Compressive Strength 160 MPaEN 993-5 1998
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.30 µm/m-°C
@Temperature 20.0 - 1000 °C
ASTM C-372
Thermal Conductivity 21.0 W/m-K
@Temperature 700 °C
Hot strip, Mean temp.; SINTEF
 28.0 W/m-K
@Temperature 500 °C
Hot strip, Mean temp.; SINTEF
 38.0 W/m-K
@Temperature 200 °C
Hot strip, Mean temp.; SINTEF
Maximum Service Temperature, Air 1580 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 + Fe2O3 + CaO 0.50 %
Si3N4 18 %
SiC 78 %
Silicon, Si 0.50 %
SiO2 + Si2ON2 2.0 %
 
Descriptive Properties
ColorGrey
Corrosion Resistance 3SINTEF
Dimensional Tolerances (Length/Width/Thickness)±2.0/±2.0/±1.0 mm
Standard Sizes510x300x50mm, 500x300x100mm, or 230x114x64mmOther sizes made on request

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
3M Techical Ceramics Ekasic® S Silicon Nitride
AISI 1040 Steel, annealed at 790°C (1450°F)
3M Techical Ceramics Ekatherm® Silicon Nitride
3M Techical Ceramics Ekasic® T Plus Silicon Carbide

CSKAM036 / 2187

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.