MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epsan Eplamid 66 GX0 25 RP Q1C5B601 Polyamide 66, Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 66 reinforced with 25% of glass fiber, heat stabilized for injection molding. Red phosphorous based, halogen free flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire at 960°C. It gives very good performance and high electrical demanding application.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmParallel; ISO 294-4
 0.0050 cm/cmNormal; ISO 294-4
Ash 25 %ISO 3451-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 150 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 9400 MPaISO 527-2
Flexural Strength 245 MPaISO 178
Flexural Modulus 8700 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VEN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 245 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75-2/A
Vicat Softening Point 250 °CISO 306/B50
Flammability, UL94 V-0
@Thickness 0.800 mm
EN 60695-11-10
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
Ravago Manufacturing Americas Hylon® N1025HLFRA Nylon 66, 25% Glass Filled, Conditioned
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
Celanese SO.F.TER Nylfor A® A2 FR1/2A Nylon 66
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned)

PEPSAN060 / 186374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.