MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Glass Fiber Reinforced

Material Notes: Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:
  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Former DSM Engineering Plastics product line is now with Envalior.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.65 g/cc0.0596 lb/in³ISO 1183
    Moisture Absorption at Equilibrium 1.2 %1.2 %Similar to ISO 62
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 180 MPa26100 psiISO 527-1/-2
    Elongation at Break 2.0 %2.0 %ISO 527-1/-2
    Tensile Modulus 14.0 GPa2030 ksiISO 527-1/-2
    Charpy Impact, Notched  0.800 J/cm²
    @Temperature -30.0 °C
    3.81 ft-lb/in²
    @Temperature -22.0 °F
    ISO 179/1eA
     0.800 J/cm²
    @Temperature 23.0 °C
    3.81 ft-lb/in²
    @Temperature 73.4 °F
    ISO 179/1eA
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 20.0 µm/m-°C
    @Temperature 20.0 °C
    11.1 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359-1/-2
    CTE, linear, Transverse to Flow 70.0 µm/m-°C
    @Temperature 20.0 °C
    38.9 µin/in-°F
    @Temperature 68.0 °F
    ISO 11359-1/-2
    Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
    Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 75-1/-2
    Flammability, UL94 V-0
    @Thickness 0.750 mm
    V-0
    @Thickness 0.0295 in
    IEC 60695-11-10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Envalior Stanyl® TS256F6 Nylon 46-30% Glass Reinforced (Asian Grade) (Dry)
    Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35

    PDSMAS006 / 31110

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.