MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Hypalon® H611 Chlorosulphonated Polyethylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
    Properties
  • Excellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.
  • CSM compounds resist fire and are self extinguishing when the flame is removed.
  • Resistance to chemicals; resistant to most inorganic chemical products, good resistance to general acids, oils and greases.

All information provided by Trelleborg

Key Words: CSM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength, Yield 8.00 MPa
Elongation at Break 350 %
Tear Strength 8.00 kN/m
Compression Set 40 %
@Temperature 70.0 °C,
Time 79200 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -35.0 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene
Trelleborg Hypalon® H606 Chlorosulphonated Polyethylene
DuPont Mobility and Materials Hypalon® 45 Chlorosulfonated Polyethylene Rubber, General Description
DuPont Mobility and Materials Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound

PTRELL152 / 83910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.