MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Data provided by the manufacturer, Dyneon LLC.

This melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of performance and processing advantages. Its thermal decomposition in air (TGA) is 420°C. It is recommended for film, tube, and profile extrusion, wire coating, and blow and injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc0.0704 lb/in³
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
20 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444ASTM D2240
Tensile Strength, Ultimate 24.1 MPa3500 psiMeasured on extruded film, ASTM D638
Elongation at Break 600 %600 %Measured on extruded film, ASTM D638
Flexural Modulus 0.0830 GPa12.0 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.6
@Frequency 1e+7 Hz
4.6
@Frequency 1e+7 Hz
 6.6
@Frequency 100000 Hz
6.6
@Frequency 100000 Hz
 
Thermal PropertiesMetricEnglishComments
Melting Point 115 - 257 °C239 - 495 °FASTM D3418
Maximum Service Temperature, Air >= 150 °C>= 302 °FE-beam cured high temperature resistance.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ THV 220G Fluorothermoplastic
3M Dyneon™ THV™ 400 Fluorothermoplastic
3M Dyneon™ THV™ 500 Fluorothermoplastic
3M Dyneon™ THV 221GZ Fluoroplastic Granules
3M Dyneon™ THV 220A Fluorothermoplastic

PDYN01 / 34696

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.