MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Refractaloy 26 Iron-Nickel Alloy (ATVS 7 Mo)
Categories: Metal; Superalloy; Iron Base

Material Notes: Typical Applications: Gas turbine parts, blades, bolts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  124 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
18000 psi
@Temperature 1500 °F,
Time 1000 hour
 186 MPa
@Temperature 816 °C,
Time 360000 sec
27000 psi
@Temperature 1500 °F,
Time 100 hour
 262 MPa
@Temperature 732 °C,
Time 3.60e+6 sec
38000 psi
@Temperature 1350 °F,
Time 1000 hour
 352 MPa
@Temperature 732 °C,
Time 360000 sec
51000 psi
@Temperature 1350 °F,
Time 100 hour
 434 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
63000 psi
@Temperature 1200 °F,
Time 1000 hour
 552 MPa
@Temperature 649 °C,
Time 360000 sec
80000 psi
@Temperature 1200 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 100 °C
7.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 15.1 W/m-K
@Temperature 20.0 - 100 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.20 %0.20 %
Carbon, C 0.030 %0.030 %
Chromium, Cr 18 %18 %
Cobalt, Co 20 %20 %
Iron, Fe 19.37 %19.37 %Balance
Manganese, Mn 0.80 %0.80 %
Nickel, Ni 38 %38 %
Silicon, Si 1.0 %1.0 %
Titanium, Ti 2.6 %2.6 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Discaloy Iron Alloy (UNS K66220)
Cast Stainless Steel HU50, UNS N08005
Carpenter Pyromet® CTX-3 Superalloy, Heat Treated
Carlson C 825 Nickel-Iron-Chromium Alloy
Carlson 330 Austenitic Alloy

NZ97061 / 191458

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.