MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Graphene Oxide (GO) Film
Categories: Carbon

Material Notes: Graphene oxide is noted for its mechanical and thermal properties. The starting material is graphite, which is chemically processed to obtain monolayer flakes of graphene oxide. The insulating film is prepared by the filtration of an aqueous monolayer graphene oxide dispersion.

Applications: Biomedical, membranes.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 12.0 - 15.0 microns
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 49 - 56 %vacuum dried aqueous dispersion
Hydrogen, H 0.00 - 1.0 %vacuum dried aqueous dispersion
Nitrogen, N 0.00 - 1.0 %vacuum dried aqueous dispersion
Oxygen, O 41 - 50 %vacuum dried aqueous dispersion
Sulfur, S 0.00 - 2.0 %vacuum dried aqueous dispersion
 
Descriptive Properties
ColorYellow-Brown
DispersibilityPolar Solvents

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Graphene Oxide (GO) Dispersion
Goodfellow Reduced Graphene Oxide (GO) Powder
Goodfellow CVD Graphene Film on Quartz Glass
Goodfellow Ultra Clean CVD Graphene Film on SiO2/Si Wafers
Goodfellow CVD Graphene Film on PET

CGOODF099m / 197459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.