MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® EP6897-61 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® EP6897-61 adhesive is a one-coat adhesive used to bond castable and RIM urethane elastomers to metal. It is composed of a mixture of polymers and curatives dissolved in an organic solvent system. Chemlok EP6897-61 adhesive is also used to bond a wide variety of both polyether and polyester castable urethanes to metal. This adhesive bonds with polyether and polyester castable urethanes of varying hardness, based on both TDI and MDI. Chemlok EP6897-61 adhesive provides bond strengths greater than the tear strength of the urethane substrate.

Features: bonds metal to a wide variety of polyether and polyester compounds include RIM urethane. requires only a single coat for most applications, minimizing application costs. dries fast to allow rapid turnaround times, reducing the number of coated parts kept in inventory. provides good cosmetics; does not interfere with aesthetics of finished part. eliminates the need to inventory several adhesives due to the adhesive’s versatility.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.40 - 7.60 lb/gal
Solids Content 20.5 - 23.5 %by weight
Brookfield Viscosity 100 - 300 cP
@Temperature 25.0 °C,
Time 20.0 - 40.0 sec
Brookfield LVT, Spindle 2, 30 rpm, Zahn Cup #3
 
Thermal PropertiesOriginal ValueComments
Flash Point 5.00 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceClear, slightly yellow liquid
SolventsMethyl Ethyl Ketone (MEK), Xylene, Dowanol BC300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9054 / 232443

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.