MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Toagosei America Aron Alpha® Industrial Krazy Glue™ 901H2 Flexible Cyanoacrylate Adhesive
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: The 900 series features heat and moisture resistance.

Information provided by Toagosei America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  1.067 g/cc
@Temperature 20.0 °C
1.067 g/cc
@Temperature 68.0 °F
Liquid
 1.214 g/cc
@Temperature 20.0 °C
1.214 g/cc
@Temperature 68.0 °F
Solid
Viscosity 5.0 cP5.0 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength 13.0 MPa1890 psivs. ABS
 25.0 MPa3630 psivs. Aluminum
 26.0 MPa3770 psivs, PVC
 30.0 MPa4350 psivs. Iron
Modulus of Elasticity 1.14 GPa165 ksi
Adhesive Bond Strength 0.600 MPa87.0 psiTensile Shear vs. Chloroprene
 0.600 MPa87.0 psiTensile Shear vs. EPDM Rubber
 7.00 MPa1020 psiTensile Shear vs. Polycarbonate
 27.6 MPa4000 psiTensile Shear vs. Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Glass Transition Temp, Tg 123 °C253 °F
Shrinkage 12.1 %12.1 %
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0167 min0.000278 hourSet Time vs. Chloroprene
 0.0167 min0.000278 hourSet Time vs. EPDM Rubber
 0.0500 min0.000833 hourSet Time vs. PVC
 0.167 min0.00278 hourSet Time vs. ABS
 0.250 min0.00417 hourSet Time vs. Steel
 0.500 min0.00833 hourSet Time vs. Aluminum
 0.500 min0.00833 hourSet Time vs. Polycarbonate
 
Descriptive Properties
ColorColorless and Transparent
Gap Fill0.004 inches
Main IngredientEthyl 2-Cyanoacrylate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARON0006 / 293908

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.