MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP76MHT Two Component, Nickel Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Good electrical and thermal conductivity
  • Superior temperature resistance
  • Convenient processing
  • Excellent dimensional stability
Product Description: Master Bond EP76MHT is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing and coating. EP76MHT is easy to use. It has a paste like consistency and the mix ratio is a forgiving one to one by weight or volume. It has an exceptionally long working life as well. It will cure readily at ambient temperatures in 3-5 days or at 200°F in 2-3 hours. The optimum cure schedule is overnight at ambient temperature followed by 3-4 hours at 150°F. EP76MHT is particularly noteworthy for its strength profile. Normally, there is a noticeable diminution of bond strength when epoxies are formulated to be electrically conductive. However EP76MHT, when fully cured, has a lap shear strength of over 2,000 psi. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, composites, vulcanized rubbers and many plastics. Furthermore, EP76MHT has high compressive strength, superb dimensional stability and has low shrinkage upon cure. Some other desirable attributes are good chemical resistance including to water, oils and cleaning agents. The service temperature range is -60°F to +400°F. Parts A and B are both gray in color. Master Bond EP76MHT is particularly useful in aerospace, electronic, electrical and other industries where nickel conductivity is desirable from a functional and cost perspective. It is especially useful in applications requiring shielding and static dissipation.

Product Advantages:

  • Convenient handling: forgiving one to one by weight or volume
  • Contains no solvents or diluents
  • Versatile cure schedules; ambient temperature cures or fast elevated temperature cures as required
  • Good electrical and thermal conductivity
  • Exceptional bond strength
  • Highly useful physical strength profile

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity >= 700000 cP>= 700000 cPPart A, thixotropic
 >= 1.00e+6 cP>= 1.00e+6 cPPart B, thixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 44.8 MPa>= 6500 psi
Tensile Modulus >= 3.45 GPa>= 500 ksi
Compressive Strength >= 152 MPa>= 22000 psi
Adhesive Bond Strength >= 14.5 MPa>= 2100 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.0 - 10 ohm-cm5.0 - 10 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C16.7 - 19.4 µin/in-°F
Thermal Conductivity 1.15 - 1.30 W/m-K7.98 - 9.02 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 85.0 - 90.0 °C185 - 194 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 4320 - 7200 min
@Temperature 23.9 °C
72.0 - 120 hour
@Temperature 75.0 °F
Working Life >= 120 min>= 120 minAfter mixing, 100 g batch
Shelf Life 3.00 - 6.00 Month
@Temperature <=23.9 °C
3.00 - 6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Cure Scheduleovernight at 75°Ffollowed by 3-4 hours at 150°F
Mixing Ratio1:1 by weight or volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
Special Metals INCOLOY® Alloy 020
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016)
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)

PMASTM900 / 185493

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.