MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Isoplast® 301 Polyurethane (PUR-RT), Clear Amorphous Polymer  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: ISOPLAST® 301 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance and toughness.

Data provided by Dow Chemical.

Lubrizol acquired the Isoplast product line from Dow in 2009.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM Data
Water Absorption 0.19 %
Linear Mold Shrinkage 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 123
Tensile Strength, Ultimate 62.1 MPaASTM Data
Tensile Strength, Yield 69.0 MPaASTM Data
Elongation at Break 140 %ASTM Data
Elongation at Yield 5.1 %ISO Data
Tensile Modulus 2.14 GPaASTM Data
Izod Impact, Notched 1.28 J/cmASTM Data
Charpy Impact Unnotched NBISO Data
 NBISO Data, Low Temp
Charpy Impact, Notched 0.500 J/cm²ISO Data, Low Temp
 1.10 J/cm²ISO Data
Impact Test 90.4 JInstrumented Dart Total Energy, 23°C. Value at -30°C is 90.4 J.
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.2 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °CUnannealed; ASTM Data
 104 °CAnnealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °CUnannealed; ASTM Data
 98.9 °CAnnealed; ASTM Data
Vicat Softening Point 109 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88 %

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Selar® PA 3426 Nylon Barrier Resin
Celanese Zytel® 101 NC010 PA66
C.O.I.M. LARIPUR® LPR72D25 Special Adipate Ester Polyurethane
BASF Ultramid® 8202 HS PA6 (Dry)
BASF Ultramid® 8202 HS PA6 (Conditioned)

PDW070 / 34301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.