MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® AT10 Nylon 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Notes: AT10 is a modified nylon 66 that offers ultra high impact strength coupled with good rigidity, with this impact resistance maintained at sub-zero temperatures; The excellent impact performance also means that it may be possible to use moldings prior to any conditioning.

Availability: Europe; North America

Features: High Rigidity; Low Temperature Impact Resistance; Ultra High Impact Resistance

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %50% RH; ISO 62
Linear Mold Shrinkage 0.020 - 0.024 cm/cm0.020 - 0.024 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 42.0 MPa6090 psiISO 527-2
Tensile Modulus 1.50 GPa218 ksiISO 527-2
Flexural Strength 30.0 MPa4350 psiISO 178
Flexural Modulus 1.10 GPa160 ksiISO 178
Izod Impact, Notched (ISO) NBNBISO 180
Izod Impact, Unnotched (ISO) NBNBISO 180
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 11.8 kV/mm
@Thickness 3.00 mm
300 kV/in
@Thickness 0.118 in
IEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FUnannealed; ISO 72-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 285 °C509 - 545 °F
Middle Barrel Temperature 265 - 285 °C509 - 545 °F
Front Barrel Temperature 265 - 285 °C509 - 545 °F
Melt Temperature <= 300 °C<= 572 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 hour2.00 hour
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0557 / 237048

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.