Uncured silicone rubber with a minimum thickness of 0.015 in.(0.38 mm) on Prime Coated 1523 Fiberglass; 0.0015 in. (0.8 mm) polyethylene interleave; overall thickness 0.030 in ± 0.003 (0.76 mm ± 0.076). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 1115 g/m² ± 50.9 (32.9 oz./yd.² ± 1.5). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Maximum Flame and Glow Time: 15 seconds. Maximum Char Length: 7.6 cm (3 in). Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |