MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mallard Creek Polymers Rovene® 4301 Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Rovene® 4301 is a self crosslinking, carboxylated styrene-butadiene emulsion that has a very stiff hand. The binder is especially recommended for durable nonwovens such as floor maintenance pads and roof shingle mats, both glass and organic. Rovene® 4301 may be further crosslinked with external resins to enhance resistance properties, such as hot elongation resistance on organic roofing mats or chemical and solvent resistance on floor maintenance pads.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 4301 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 49 - 51 %49 - 51 %
Particle Size 0.14 µm0.14 µm
pH 8.5 - 9.28.5 - 9.2
Brookfield Viscosity <= 750 cP<= 750 cP#20/200
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 58.0 °C136 °F
 
Descriptive Properties
EmulsifiersAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMCP122 / 157399

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.