MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials Infino® SA-1100 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: General, Switch, Breaks

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0046 - 0.0056 cm/cm
@Thickness 3.20 mm
0.0046 - 0.0056 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0048 - 0.0058 cm/cm
@Thickness 3.20 mm
0.0048 - 0.0058 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 65.7 MPa9530 psi50 mm/min; ASTM D638
Tensile Strength, Yield 63.7 MPa9250 psi50 mm/min; ASTM D638
Elongation at Break 91 %91 %50 mm/min; ASTM D638
Tensile Modulus 2.01 GPa292 ksi50 mm/min; ASTM D638
Flexural Strength 96.1 MPa13900 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.26 GPa327 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  1.96 J/cm
@Thickness 6.35 mm
3.67 ft-lb/in
@Thickness 0.250 in
ASTM D256
 6.86 J/cm
@Thickness 3.17 mm
12.9 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VPLC 3; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 6.40 mm
261 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 142 °C288 °FB/50; ISO R 306
Flammability, UL94 V-2
@Thickness 1.50 - 3.00 mm
V-2
@Thickness 0.0591 - 0.118 in
Glow Wire Ignition Temperature 875 °C
@Thickness 1.50 mm
1610 °F
@Thickness 0.0591 in
IEC 60695-2-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® HN-3104 PC, 10% Glass Filled FR
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
Covestro Makrolon® 6557 Polycarbonate, Injection Grade
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release

PLOTT9864 / 205726

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.